Sealing and bearing position repairs

Here we have a slideshow with more information about layer modes and sealing surefaces

2014-06-18 11.26.48

A bearing surface is oval worn. Plated on site to correct dimensions.

2014-06-18 18.43.55

The surface is finished and a top layer of nickel is added.

2014-07-02 08.28.48

Sealing faces of gas turbine house plated with copper and then sanded down to the correct tolerance.

2014-07-06 16.39.15

Corrosions damage where the steam has destroyed the sealing surface and which now is repaired with a hard copper that is 250 Brinell. Now it is plated a dense top layer with nickel so no new corruption will occur.